Abstract
Using an AFM-based instrumented nanoindentation system, the nanoindentation response of γ' particles (Ni3Al) in a Ni-base single crystal superalloy CMSX-4 was characterized to demonstrate the influence of the softer γ matrix on the measurement of nano-mechanical properties of γ' particles. The properties of the γ' particles were measured after both a standard and a coarsening heat treatment, in which the initially sub-micron sized cuboidal γ' particles transformed to large, irregularly shaped γ' precipitates with dimensions in excess of 30 μm. The measured nano-hardness of the coarsened γ' precipitates in CMSX-4 appears to increase slightly with the increasing load. Nano-compression testing of cuboidal γ' particles, electrolytically extracted from a CMSX-4 after a standard solution and age heat treatment, was also performed. With a maximum value of 10 GPa, the measured yield stress of these dislocation-free γ' particles approaches the ideal strength and is equivalent to -G/17. Compared to the measured yield strengths of γ' phase in its bulk crystal form, these nano-compression results are more than a factor of 33 higher. Additionally, the 'softening' effect of Ga+ ion implantation on the strength of dislocation-free nanocrystals was also assessed. The resulting yield strengths of cuboidal γ' precipitates imaged with a focused ion beam were at least 5 GPa lower than those that had not been subjected to Ga+ ion implantation.
| Original language | English (US) |
|---|---|
| Title of host publication | Superalloys 2012 |
| Publisher | John Wiley and Sons |
| Pages | 83-91 |
| Number of pages | 9 |
| ISBN (Print) | 9780470943205 |
| DOIs | |
| State | Published - Oct 2 2012 |
| Externally published | Yes |
Keywords
- γ′ precipitate
- Nano-compression
- Nanoindentation
- Superalloy
ASJC Scopus subject areas
- General Materials Science
Fingerprint
Dive into the research topics of 'Nanoindentation and Nano-Compresion Testing of Ni3Al Precipitates'. Together they form a unique fingerprint.Cite this
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS