Skip to main navigation Skip to search Skip to main content

High temperature nanoindentation of a Re-bearing single crystal Ni-base superalloy

Research output: Contribution to journalArticlepeer-review

Abstract

Nanoindentation studies of single crystal Ni-base superalloy CMSX-4 oriented in the 〈0 0 1〉 and 〈1 1 0〉 directions were conducted over a range of temperatures from 303 to 673 K. The creep compliance at peak load was measured at each of the test temperatures and incorporated into the contact mechanics analyses to calculate the elastic modulus of CMSX-4 as a function of temperature. The measured variations in hardness and modulus as a function of temperature determined via nanoindentation are consistent with previously reported values.

Original languageEnglish (US)
Pages (from-to)275-278
Number of pages4
JournalScripta Materialia
Volume58
Issue number4
DOIs
StatePublished - Feb 2008

Keywords

  • High temperature deformation
  • Nanoindentation
  • Nickel alloys

ASJC Scopus subject areas

  • General Materials Science
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering
  • Metals and Alloys

Fingerprint

Dive into the research topics of 'High temperature nanoindentation of a Re-bearing single crystal Ni-base superalloy'. Together they form a unique fingerprint.

Cite this