Galvanic corrosion between copper and tantalum under CMP conditions

Subramanian Tamilmani, Wayne Huang, Srini Raghavan

Research output: Contribution to journalArticlepeer-review

29 Scopus citations

Fingerprint

Dive into the research topics of 'Galvanic corrosion between copper and tantalum under CMP conditions'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemical Compounds